2013
R A Hernandez Hernandez, F Legorreta Garcia, L E Hernandez Cruz, A Martinez Luevanos, ?Iron removal from a kaolinitic clay by leaching to obtain high whiteness index? (2013) IOP Conf. Series: Materials Science and Engineering 45 (2013) 012002 doi:10.1088/1757-899X/45/1/012002
Abstract
Beige kaolin clays were crushed and sieved. The mineral was characterized by X-ray diffraction and chemically analyzed by atomic absorption spectrophotometry. The material below 37 microns was leached with oxalic acid. A study of main variables of the leaching process in different ranges was realized: time (0 to 120 min), temperature (25 to 100 C) and acid concentration (0.01 to 0.5 M). Crystallographic analysis of the initial sample indicates the presence of kaolinite, iron oxides in the form of magnetite and iron-titanium oxides. By this method it was possible to obtain iron extraction percentages over 80% and whiteness index above to 90%.
Purificación del caolín por electrólisis
SEPARACIÓN DE ÓXIDOS DE Fe DEL CAOLÍN POR SIMPLE ASENTAMIENTO
PURIFICACIÓN DE CAOLÍN POR ELECTRÓLISIS
ESTUDIO DE LA MANGANITA EuxCa1-xMnO3
ESTUDIO DE LA MANGANITA EuxCa1-xMnO3
BLANQUEO DE ARCILLAS CAOLINÍTICAS COLOR CAFÉ POR DISPERSION Y ASENTAMIENTO