Román Ángel Hernández Hernández, Felipe Legorreta García, Leticia Esperanza Hernández Cruz, and Antonia Martínez Luévanos, ?Statistical Treatment of Bleaching Kaolin by Iron Removal?, J. Mex. Chem. Soc. (2013), 57(4), 261-266. ISSN:1870-249X
Abstract
Abstract. In the present study, oxalic acid was used as a leaching reagent to remove iron from a kaolin mineral. Statistical analysis was conducted to determine the most influential factors in the dissolution of iron from the kaolin mineral. Our goal was ferric iron solubilization and its reduction to ferrous iron to improve the iron removal in theacid medium. Leaching experiments were conducted at atmospheric pressure. A two-level factorial design of the type 24 was utilized. The dependent variable was the percentage of dissolved iron, and the dependentvariables in this study were acid concentration (0.35 and 0.50 M), temperature (75 C and 100 C), leaching time (2 and 4 h), and pH (1.5 and 2.5). An analysis of variance revealed that the effects of the factors temperature (b), pH (d), and the combined effects of temperature and time (bc) resulted in the maximum dissolution of iron of 88%at 100 C, giving a kaolin mineral with a whiteness index 93.50%.
BLANQUEO DE ARCILLAS CAOLINÍTICAS COLOR CAFÉ POR DISPERSION Y ASENTAMIENTO
ESTUDIO DE LA MANGANITA EuxCa1-xMnO3
BLANQUEO DE ARCILLAS CAOLINÍTICAS COLOR CAFÉ POR DISPERSION Y ASENTAMIENTO
Purificación del caolín por electrólisis
SÍNTESIS Y CARACTERIZACIÓN DE CaMnO3 DOPADA CON LANTANO OBTENIDA MEDIANTE EL MÉTODO DE COMBUSTIÓN
SÍNTESIS Y CARACTERIZACIÓN DE CaMnO3 DOPADA CON LANTANO OBTENIDA MEDIANTE EL MÉTODO DE COMBUSTIÓN
OBTENCIÓN DE POLVOS CERÁMICOS DEL SISTEMA EuxCa1-xMnO3 POR EL MÉTODO POLIOL